3. Prepare aluminum alloy filler metal by powder metallurgy




3.1 Experimental materials and methods




Set the granularity to 45? 105 ^m A1-Si filler metal powder and size of 25? The powder of 45 KAlF4 flux is uniformly mixed according to the mass ratio of 9:1, and pressed into a quasi-40mm cylinder powder on a cold isostatic press with a unit pressing pressure of 100? 300MPa. Then in a vacuum sintering furnace with a vacuum degree of 10-3Pa, 300? Sintering 2h at 550 °C and cooling to room temperature. Then the sintered blank was extruded with loot hot extruder at extrusion ratio of 64:1, extrusion speed of 2.2m/min and extrusion temperature of 400°C. Density was measured by drainage method. After the metallographic samples were mechanically polished and etched with standard Keller reagent (0.5% HF+1.5% HC1+2.5%HNO3+95.5%H2O), the microstructure of the materials before and after hot extrusion was observed by scanning electron microscopy (SEM) QUANTA200.




3.2 Experimental Conclusion




(1) The size of the pressing force determines the density of the self-brazing aluminum filler metal powder, the higher the pressing force, the higher the density of the powder. When the pressing pressure is low, the density of billet increases rapidly with the increasing of pressing force. When the pressing force is high, the density increases slowly with the increase of pressure. When the pressing force is about 150MPa, the relative density of the powder billet can reach 80%, and the powder billet has the conditions for subsequent sintering and hot extrusion.




(2) The conventional sintering process (including vacuum sintering) can not improve the density of self-brazing aluminum filler metal powder billet, lower than the solid phase line temperature sintering, the density of the sample not only did not increase, but decreased; When sintering at a temperature higher than the solidus line, the sample will melt. Moreover, the sintering density of powder billet will not increase with the increase of sintering temperature.




(3) In the process of hot extrusion, plastic deformation occurs in the sintered billet, the void and boundary between the internal particles disappear, the cavity decreases, and the relative density of the sample reaches 96.7%. In terms of phase composition, the white particles KAlF4 and the fine black spots Si are dispersed uniformly on the A1-Si matrix.






Porous metal foam has many physical properties such as porosity, vibration reduction, damping, sound absorption, sound insulation, heat dissipation, shock energy absorption, electromagnetic shielding, etc. Therefore, it has been more and more widely used in general industrial fields and high-tech fields at home and abroad. At present, the research on porous metal foam is mostly carried out by metallurgy or metal materials workers using the single-discipline method, and the research on porous metal foam should be based on the integration of multiple disciplines and multiple knowledge, and it is difficult to make breakthrough progress in single-discipline research, and it should be separated from application. In the future, multi-disciplinary penetration should be adopted to overcome the disconnection between material preparation and application, and targeted research should be carried out on the basis of demand, so as to speed up the process of transforming science and technology into real productivity.


Add: No. 98 Lushan Road, Lianxi District, Jiujiang City, Jiangxi China.

Tel: 0086 13560461580

Email sales@yaray.com.cn

Business

News

About Us

Telephone
E-MAIL
Contact Us:
18979290830
No content
Word 500(limit 500 Character)
Technical Support: CLOUD | Admin Login
seo seo
×